Materials

Tempered Glass Enamel

Date Time:2019-11-11 21:19:56Visited:1474

Tempered Temperature: 680-720

Firing Temperature: 600-650℃

Coefficient Of Thermal Expansion (CTE): (75-95)x10-7/k (50-300℃)

Acid And Alkali Resistance:

Acid Resistance: No sharp trace on the surface after dipping in 3.5% hydro choric acid solution for 10-15 min at room temperature

Alkali Resistance: No sharp trace on the surface after dipping in 10% caustic soda solution for 10-15 min at room temperature

Supply Mode: powder, printing enamel